Orca Slicer Calibration Tests In Order

The calibration menu is the reason most people move to Orca Slicer, and it is the part of Orca Slicer that repays attention fastest. Every test below is generated by the software, printed by your machine and read by you in a couple of minutes.

Run the Orca Slicer tests in the order given. Each test assumes the one before it is already correct, so jumping ahead produces numbers that shift under you later.

Last updated 28 November 2026. Written against Orca Slicer 2.5.2.

Why Order Matters

In Orca Slicer, temperature affects how much plastic flows. Flow affects how corners look. Corners are what pressure advance is measuring. So temperature first, flow second, pressure advance third. Orca Slicer lists them in this order in the menu for exactly this reason, and skipping around is the most common way people end up recalibrating everything twice.

Before any of it, make sure your bed is level and your Z offset is right. Those are firmware jobs, not Orca Slicer jobs, and no amount of slicer calibration fixes a first layer that is crushed or floating.

Test One: Temperature Tower

What this Orca Slicer test fixes: weak layer bonding, stringing, and the guesswork in the range printed on the filament box.

3D printed temperature tower with five test blocks

How to run it: open Calibration, choose Temperature, pick your filament, and Orca Slicer builds a tower where each block prints at a different temperature. It changes the temperature mid print automatically, so you print once and get the whole range.

How to read the Orca Slicer result: look for the block with the cleanest overhangs and the least stringing between the pegs, then check layer bonding by trying to snap each block. The best block is usually a compromise between the two, and leaning a few degrees hotter is safer for strength.

Test Two: Flow Rate

What this Orca Slicer test fixes: rough top surfaces, gaps between lines, bulging corners, dimensions that come out slightly large.

Four flow rate test squares ranging from under to over extruded

How to run it: Orca Slicer splits this into a coarse pass and a fine pass. The coarse pass prints squares from minus 20 to plus 20. Pick the smoothest, enter the value, then run the fine pass, which prints a narrower range around your choice.

How to read the Orca Slicer result: look across the top surface of each square under good light. You want the one with no gaps between the extrusion lines and no raised ridges. Ridges mean too much flow, gaps mean too little. Save the result into the filament profile rather than the process profile, because flow is a property of the material.

The arithmetic is where people come unstuck, because the number printed on the square is not the number you type in. That figure is a modifier, not the flow ratio itself. Take your current flow ratio, which is 1 on most stock profiles, multiply it by one hundred plus the modifier, then divide by one hundred. A modifier of minus 5 on a stock profile gives 1 multiplied by 95, divided by 100, so 0.95. Enter that, then run the fine pass against it. If the fine pass comes back at plus 2, the sum is 0.95 multiplied by 102, divided by 100, which is 0.969. Skipping that second calculation is the single most common calibration mistake, and it leaves you with a value that is close but never quite right.

You enter the finished figure in the filament profile under Filament, as Flow ratio. Save the profile under your own name rather than overwriting the stock one, so you can always get back to a known starting point if a later change makes things worse.

Test Three: Pressure Advance

What this Orca Slicer test fixes: bulges on the outside of corners, thin patches coming out of them, and inconsistent extrusion when the nozzle changes speed.

Pressure advance test plate showing sharp and blobbed corners

How to run it: Orca Slicer offers three methods. The line method prints a series of lines at increasing values and is quickest. The pattern method is more precise and takes longer. The tower method sits between them. Start with the line method.

How to read the Orca Slicer result: find the line where the corners are sharpest, with no blob on the outside and no gap on the inside. Read the value from the scale printed alongside. Klipper users should note that Orca Slicer can write this value into the G-code directly, so the slicer and firmware stop disagreeing.

Test Four: Retraction

What this Orca Slicer test fixes: stringing and wisps between separate parts on the plate.

Retraction test with fine plastic wisps between two pegs

How to run it: the Orca Slicer retraction test prints a pair of towers with the retraction length stepping up as it climbs.

How to read the Orca Slicer result: find the height where strings stop appearing between the towers, and read off the corresponding length. Direct drive extruders usually settle between 0.4mm and 1mm. Bowden setups need far more, commonly 3mm to 6mm. If stringing persists at high retraction values, the problem is temperature rather than retraction, so go back to the tower.

Test Five: Max Volumetric Speed

What this Orca Slicer test fixes: prints that run slower than the speed you set, and under extrusion that appears only at high speed.

How to run it: Orca Slicer prints a model that accelerates the flow rate continuously as it rises.

How to read the Orca Slicer result: find the height where the extrusion becomes inconsistent or the surface goes rough, and read the volumetric flow at that point. Set your filament profile for that machine slightly below it. This single number is why a print set to 300mm per second finishes at nothing like that speed, because Orca Slicer throttles to protect the hot end rather than letting it skip.

Optional: Tolerance And VFA

The Orca Tolerance Test prints pins and sockets at varying clearances, which tells you what gap to design into parts that must fit together. Useful once, then written down forever.

The VFA test targets vertical fine artefacts, the faint banding on flat walls caused by motor resonance. Run it only if you can already see that banding, because the fix is usually hardware rather than Orca Slicer.

Saving Your Results

Flow rate, pressure advance, temperature and retraction all belong in the filament profile. They are material properties, so saving them there means every print with that spool inherits them automatically.

After finishing a calibration run, start a new project. Orca Slicer stays in calibration mode until you do, and people regularly slice a real part while still in that mode and wonder why the result is strange.

How Often To Recalibrate

Run the Orca Slicer suite once per filament, not once per print. A new brand or a new colour from the same brand is worth a flow test, because pigment changes flow behaviour more than people expect. A new spool of something you have already calibrated usually needs nothing.

Recalibrate Orca Slicer after hardware changes too. A new nozzle, a new hot end or a new extruder resets the assumptions behind every Orca Slicer number you saved.

Reading A Test That Failed

Not every Orca Slicer calibration print gives a clean answer, and a failed test is information rather than a waste of filament.

If every block on a temperature tower looks equally bad, the problem is upstream of temperature. Check that the filament is dry, because wet filament produces stringing and poor surfaces at every temperature and will defeat the whole Orca Slicer calibration sequence.

If a flow rate test shows no clear best square, your first layer may be the culprit. A squashed or lifted first layer distorts the squares above it. Fix Z offset, then run the Orca Slicer flow test again.

If pressure advance results look identical across the range, check that the test actually applied. Orca Slicer needs the correct filament selected before generating the test, and running it against the wrong profile produces a print that tells you nothing.

New Printer Or New Filament

The two situations need different amounts of work, and treating them the same wastes hours.

A new filament needs temperature, flow rate and pressure advance. That is three Orca Slicer tests and about an hour including print time. Retraction only needs revisiting if you see stringing.

A new printer needs all of the above plus max volumetric speed, and it needs the hardware side checked first. Bed level, Z offset and extruder steps are firmware calibrations, and Orca Slicer cannot compensate for any of them. Get those right, then run the Orca Slicer suite.

A new nozzle counts as a new printer for this purpose. Changing diameter changes flow behaviour completely, and every saved Orca Slicer value was measured against the old one.

What Calibration Will Not Fix

Orca Slicer calibration tunes the relationship between the slicer and your machine. It does nothing about mechanical problems, and a lot of frustration comes from expecting otherwise.

  • Layer shifts, which are belts, pulleys or a stepper driver overheating
  • Z banding, which is a bent lead screw or binding on the Z axis
  • Ringing and ghosting, which is frame rigidity and input shaping
  • Clogs mid print, which is heat creep or wet filament
  • Parts lifting at the corners, which is bed adhesion and enclosure temperature

If a symptom persists at every value an Orca Slicer test produces, it is mechanical. The calibration result is telling you that the slicer is not the variable.

A Worked Example

Say a new spool of PETG is stringing badly and top surfaces look rough. The Orca Slicer sequence handles this in order.

Run the temperature tower first. PETG often prints better 10 to 15 degrees below the figure on the box, and dropping temperature alone usually removes most of the stringing. Note the best block.

Run flow rate next with that temperature applied. Rough top surfaces are almost always flow, and the Orca Slicer coarse and fine passes together will land you within a percent.

Run pressure advance third. By now the corners are the only thing left looking wrong, and this is the test that fixes them.

Only if stringing survives all three is retraction worth touching. In practice, Orca Slicer users chasing PETG stringing find it was temperature about eight times out of ten.

Keeping A Record

Save each result into the filament profile and name the profile after the actual spool, not the material. PETG is not a setting. Overture PETG Black is a setting, because the next brand will behave differently.

Export your Orca Slicer configuration bundle occasionally. It is a single file holding every calibrated profile, and it means a reinstall or a new computer costs you minutes rather than another evening of test prints.

Scroll to Top